Analysis and influence of low voltage in lithium battery formation process
264 2025-04-02
First, the common reasons for poor low voltage
1. Problems related to the electrolyte
Decomposition or volatilization: The electrolyte concentration is too high, impurities (such as metal ions), or the temperature is out of control, resulting in decomposition, and gases (such as CO?, Li?CO?) to increase the internal resistance and reduce the voltage.
Poor infiltration: the viscosity of the electrolyte is too high or the proportion of additives is unbalanced, resulting in uneven wetting of the electrode material, a decrease in the utilization rate of active substances, and an increase in resistance during charging and discharging.
2. The electrode material is defective
Poor uniformity: positive and negative powder agglomeration, uneven coating thickness, resulting in local active substances can not fully react, uneven voltage distribution.
Fluid contamination/oxidation: aluminum foil/copper foil surface oxidation or foreign body attachment, increase contact resistance, hinder electron transmission.
3. Improper process parameters
Abnormal current density: excessive current causes local overheating and accelerates electrolyte decomposition; Too low current results in incomplete formation and defects of SEI film.
Voltage curve control error: wrong cut-off voltage setting (too high resulting in lithium evolution, too low resulting in capacity loss).
4. Equipment and environmental factors
Poor sealing: leakage in the formation cabinet leads to electrolyte volatilization or moisture intrusion, destroying the SEI film.
Temperature management failure: The accuracy of the temperature sensor is insufficient or the heating/cooling system is faulty, causing local temperature difference abnormalities and affecting the reaction rate.
Excessive humidity: Environmental moisture causes water molecules to embed in the graphite layer and react with lithium ions to form LiOH·nH?O, irreversible capacity loss.
5. Structural defects
Internal short circuit/diaphragm damage: dislocation of the pole plate and pinholes in the diaphragm during assembly lead to current short circuit and increased energy loss.
Poor packaging: the shell is not tightly sealed, the electrolyte leaks or gas escapes, and the internal pressure of the battery cell is unbalanced.
Second, the impact of low voltage on the battery cell
1. Capacity and energy density decrease
The utilization rate of active substances is low (such as poor electrode infiltration areas), the effective storage of lithium is reduced, and the nominal capacity cannot reach the design value.
SEI film defects lead to the obstruction of lithium ion transport, and the capacity attenuation accelerates during the cycle.
2. Shortened cycle life
Local lithium evolution or dendrite growth punctures the diaphragm, triggering an internal short circuit and increasing the risk of thermal runaway.
Continuous decomposition of electrolyte results in thickening of solid electrolyte interface (SEI) layer, accumulation of internal resistance, and decrease of charge and discharge efficiency.
3. Potential security risks
Gas precipitation leads to cell expansion and shell bulge, which may break or leak in serious cases.
Under the condition of high internal resistance, the temperature of high current discharge increases sharply, and the risk of thermal management failure increases.
 
4. Poor consistency
The proportion of low-voltage cells between batches increases, affecting the voltage balance of modules/battery packs and reducing system reliability.

Third, solutions and preventive measures
1. Optimize the electrolytic liquid system
Choose low viscosity, high ionic conductivity electrolyte (such as LiFSI based solvent).
Control the impurity content (metal ions ≤1ppm), add stable additives (such as VC, DTD).
2. Improve electrode preparation process
Ultrasonic dispersion and ball milling were used to improve powder dispersion and reduce agglomeration.
Optimize coating parameters (such as coating speed, oven temperature) to ensure uniform electrode thickness.
Clean collector surfaces (e.g. plasma treatment) to reduce contact resistance.
3. Fine process control
Step control of formation current (such as 0.1C precharge →0.2C constant current) to avoid overreaction.
The cutoff voltage is precisely controlled in combination with the CCCV mode (e.g. ternary material 4.25V vs graphite 3.65V).
4. Upgrade the environment and devices
Use a clean workshop environment with humidity ≤1%RH and temperature 25±2℃.
Equipped with constant temperature forming cabinet (±0.5℃ accuracy) and online gas detection system.
5. Quality monitoring and feedback mechanism
Implement real-time monitoring of the formation process (such as voltage-time curve analysis) to screen abnormal cells.
In situ testing (e.g. XRD, EIS) was used to locate the defect root and iterate the process parameters.
summarize:
The low voltage of the forming process is mainly caused by the synergistic effect of electrolyte, electrode material, process parameters and environment, which directly affects the capacity, life and safety of the cell. By systematically optimizing materials, processes and equipment, and establishing a closed-loop quality control system, the consistency and performance of cells can be significantly improved.
主站蜘蛛池模板: 日韩av无码一区二区三区不卡| 国产精品一区二区在线蜜芽tv| 99热精品久久只有精品| 亚洲国产丝袜精品一区| 无码人妻人妻经典| 日韩中文无码有码免费视频| 国产偷国产偷亚洲清高app| 热re99久久精品国99热| 免费大黄网站在线观| 久久er99国产精品免费| 中文字幕丝袜第1页| 亚洲国产成人久久一区| 最新精品香蕉在线| 少妇熟女高潮流白浆| 人妻精品国产一区二区| 亚洲成av人不卡无码影片| 欧美亚洲日本日韩在线| 精品国产乱码一区二区三区| 国产美女遭强被高潮网站| 少妇性l交大片欧洲热妇乱xxx| 国产亚洲精品aa片在线观看网站| 97在线视频人妻无码| 2021精品国产自在现线看| 又色又爽又黄的视频网站| 亚洲成国产人片在线观看| 一区二区精品视频日本| 色欲综合久久躁天天躁蜜桃| 国产男女猛烈视频在线观看| 国产99久久九九精品无码| 国产一区二区在线影院| 亚洲日本va在线视频观看| 国产精品videossex久久发布| 亚洲日韩av片在线观看| 久久人妻精品白浆国产| 免费网站内射红桃视频| 99久久精品国产免费| 果冻传媒mv免费播放在线观看| 国产午夜成人精品视频app| 黑人大战欲求不满人妻| 狠狠久久永久免费观看| 18禁超污无遮挡无码免费动态图|